第13回
PD 資格試験開始から 10 年の実施状況
著者:
渡辺 恵司,Keiji WATANABE,林 山,Shan LIN,東海林 一,Hajime SHOHJI,太田 丈児,Joji OHTA
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced performance demonstration examinations (PD examination) for flaw depth sizing of austenitic stainless steel pipes in March 2006. At the end of FY 2015, 44 examination sessions have been completed and 58 candidates have passed the examination. The total number of PD examinee including re-tests and re-certification was 104. Passed candidates can perform depth sizing of SCC flaws with a high level of accuracy during ...
英字タイトル:
Implementation report for 10 years after the start of Japanese performance demonstration examination
第11回
PD 資格試験開始から 8 年の実施状況
著者:
渡辺 恵司,Keiji WATANABE,東海林 一,Hajime SHOHJI,秀 耕一郎,Koichiro HIDE
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced Per formance Demonstration examinations for flaw depth sizing of austenitic stainless steel pipes n March 2006. At the end of FY 2013, 40 examination sessions have been completed and 49 cand ates have passed the examination. The total number of tests administered including re-tests and re-certification was 95. It was noted that the final call for the crack length (PD examin ation answer) was adopted the phased array m...
英字タイトル:
Implementation status for eight years after the start of PD qualification examination in Japan
第8回
PD 資格試験開始から5年の実施状況
著者:
渡辺 恵司,Keiji WATANABE,東海林 一,Hajime SHOHJI,秀 耕一郎,Koichiro HIDE
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced Performance Demonstration examina tions for flaw depth sizing of austenitic stainless steel pipes in March 2006. As of February, 2011, 29 examination courses have been completed and 38 out of 49 candidates passed the examination including recertification test. The average error mar gin of the successful applicant of the PD examination to the eleventh stage was 0.31 mm, and standard deviation was 1:9 mm....
英字タイトル:
Report on Performance Demonstration test for depth sizing of SCC in austenitic stainless steel pipes during five years
第9回
PD 資格試験開始から6年の実施状況
著者:
渡辺 恵司,Keiji WATANABE,東海林 一,Hajime SHOHJI,秀 耕一郎,Koichiro HIDE
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced Performance Demonstration examin ations for flaw depth sizing of austenitic stainless steel pipes in March 2006As of January, 2012, 34examination courses h ave been completed and 37out of 47candidates passed the examination including recertification test. The average error marg in of the successful applicant of the PD examination to the eleventh stage was 0.32mm, and standard deviation was 1.93mm....
英字タイトル:
Report on Performance Demonstration for depth sizing of SCC in austenitic stainless steel pipes
第10回
PD 資格試験開始から7年の実施状況
著者:
渡辺 恵司,Keiji WATANABE,東海林 一,Hajime SHOHJI,秀 耕一郎,Koichiro HIDE
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced Performance Demonstration examinations for flaw depth sizing of austenitic stainless steel pipes in March 2006. As of January 2013, 37 examination sessions have been completed and 44 candidates have passed the examination. The total number of tests administered including re-tests and re-certification was 89. It was noted that depth sizing using a phased array plus the manual UT technique was the procedure most use...
英字タイトル:
Report on Japanese Performance Demonstration examinations For depth sizing of SCC in austenitic stainless steel pipes
第12回
PD 資格試験開始から9 年の実施状況
著者:
渡辺 恵司,Keiji WATANABE,東海林 一,Hajime SHOHJI,秀 耕一郎,Koichiro HIDE,太田 丈児,Joji OHTA
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced Performance Demonstration examinations for flaw depth sizing of austenitic stainless steel pipes in March 2006. At the end of FY 2014, 42 examination sessions have been completed and 53 candidates have passed the examination. The total number of tests administered including re-tests and re-certification was 99. Passed candidates can perform depth sizing of IGSCC flaws with a high level of accuracy. For the final d...
英字タイトル:
Current status for nine years after the start of PD qualification examination in Japan
第16回
PD資格試験実施から13年の実施状況
著者:
渡辺 恵司,東海林 一,(電中研)
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced performance demonstration examinations (PD examination) for flaw depth sizing of austenitic stainless steel pipes in March 2006. At the end of FY 2018, 50 examination sessions had been completed and 68 candidates had passed the examination. The total number of PD examinee including re-examination and re-certification was 116. Passed candidates can perform depth sizing of SCC flaws with a high level of accuracy. Mean of...
英字タイトル:
Current status of Japanese PD examination for 13 years
第17回
PD資格試験実施から15年の実施状況
著者:
渡辺 恵司,林 山,東海林 一,(電中研)
発刊日:
公開日:
キーワードタグ:
The PD Center of Central Research Institute of Electric Power Industry (CRIEPI) commenced performance demonstration examinations (PD examination) for flaw depth sizing of austenitic stainless steel pipes in March 2006. At the end of FY 2020, 54 examination sessions had been completed and 72 candidates had passed the examination. The total number of PD examinee including re-examination and re-certification was 124. Passed candidates can perform depth sizing of SCC flaws with a high level of accuracy. As a re...
英字タイトル:
Current status of Japanese PD examination for 15 years
第7回
PD資格試験開始から4年の実施状況
著者:
秀 耕一郎,Koichiro HIDE,笹原 利彦,Toshihiko SASAHARA,直本 保,Tamotsu JIKIMOTO,渡辺 恵司,Keiji WATANABE
発刊日:
公開日:
キーワードタグ:
The PD Center at the Central Research Institute of Electric Power Industry (CRIEPI) commenced Performance Demonstrat ion examinations for flaw depth sizing of austenitic stainless steel pipes in March 2006. As of April, 2010, 26 exam ination courses have been completed and 31 out of 43 candidates passed the examination. The average error margin of the successful applicant of the PD examination to the seventh stage was 0.17 mm, and standard deviation was 2.0 mm....
英字タイトル:
Report on Performance Demonstration for depth sizing of SCC flow in austenitic stainless steel pipes
第10回
WOLおよびDMW PD資格試験の実施方法について
著者:
秀 耕一郎,Koichiro HIDE,渡辺 恵司,Keiji WATANABE
発刊日:
公開日:
キーワードタグ:
In Japan, the 1st Performance Demonstration (PD) qualification examination started in March of 2006 and was operated by the Performance Demonstration (PD) center of Central Research Institute of Electric Power Industry (CRIEPI). The first application of Japanese PD system is crack depth sizing on stainless steel piping welds. PD center is planning to start weld overlay (WOL) PD examination as a second step, and dissimilar weld (DMW) PD examination as third step. In particular, WOL PD examination includ...
英字タイトル:
The examination system for Japanese WOL and DMW PD qualification test 東海林 一 Hajime SHOHJI